Chipboards with reduced consumption of urea-formaldehyde oligomers
Purpose: for use in the production of cabinet furniture, in residential and civil construction
Indicators | The values |
Density, kg / m3 | 700-800 |
Flexural strength, MPa | 19.0-21.0 |
Swelling in thickness,% no more | 22.0 |
Free formaldehyde content, mg / 100 g of board | 6-8 |
Advantages compared to analogues: the technology allows to reduce by 20% the consumption of urea-formaldehyde oligomers during their production due to the use of native potato starch modified by fermentation in the composition
Form of intellectual property protection: patent 10434 RB “Composition for chipboard”
Proposals for cooperation with investors: a contract for the implementation of work on the implementation of the developed technology or its individual solutions for other enterprises producing particle boards